CFR (Exclude Insurance) Surabaya, Indonesia main ports
Quality
The yield strength (ReH) shall minimum 170 MPA - 285 MPa; the tensile strength (Rm) shall be strictly controlled within 330 MPa; and the elongation after fracture (A) shall be guaranteed to be 20% or higher. With regard to the control of chemical composition through smelting analysis, the carbon (C) content is capped at 0.08%, the manganese (Mn) content is limited to a maximum of 0.45%, whilst harmful elements such as phosphorus (P) and sulphur (S) are strictly restricted to 0.035% or less.